http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011173892-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5423f1ced75d7fb71b03cac90433e0d3 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61Q11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K8-25 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B33-193 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61Q11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K8-25 |
filingDate | 2011-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bfde87761e04269dfc25d87591f9dadf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8e9262719fcdd15c63ca2fcb3878df2c |
publicationDate | 2011-09-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2011173892-A |
titleOfInvention | Highly cleanable silica material and dentifrice containing the same |
abstract | Disclosed is a gel / precipitated silica composite material having excellent thickening and polishing properties, and a dentifrice formulation containing the composite material. The composite material comprises 5-50% by volume silica gel, the composite material exhibits linseed oil absorption in the range of 40-100 ml / 100 g, and the composite material is in the range of 5-30 mg loss / 100,000 revolutions. A composite material exhibiting% Brass-Einlehner hardness and a dentifrice formulation containing the composite material. The composite material is preferably in the form of particles exhibiting a median particle size of 3-20 μm. [Selection figure] None |
priorityDate | 2004-11-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |