Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8fb9f44db08d1c42a53f3d28eaae416f |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-40 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K105-16 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-78 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B7-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B7-92 |
filingDate |
2010-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_873f369232762cdb882cc37ddac44271 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ec8b4ccaa5127cb8c8a49cbed8a75731 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6c3cdd03ae1600d359c955988a012567 |
publicationDate |
2011-08-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2011152787-A |
titleOfInvention |
Method for producing polylactic acid resin composition |
abstract |
Disclosed is a method for producing a polylactic acid resin composition that provides a molded article having excellent color tone and having both strength and flexibility, and an injection molded article of a polylactic acid resin composition obtained by the production method. Providing a manufacturing method of A raw material for a polylactic acid resin composition containing polylactic acid resin and cellulose having a crystallinity of less than 50% is melted using a melt kneading apparatus having a kneading screw having a screw diameter of D (mm). A method for producing a polylactic acid resin composition comprising a step of kneading to obtain a melt-kneaded product, wherein the melt-kneading is performed at a temperature of the melt-kneaded product T (° C.), and the melt-kneaded product discharge amount of the melt-kneading device W (kg / h), and the rotational speed of the kneading screw is R (r / min), and the polylactic acid resin includes a step of satisfying the following formulas (1) and (2) A method for producing the composition. 170 ℃ ≦ T ≦ 220 ℃ (1) 0.15 ≦ (W × 100) / (D × R) ≦ 4.0 (2) [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021149524-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015531320-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2013099770-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013151661-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013151636-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7135222-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022163117-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10093798-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11634559-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112063141-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112063141-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/IT-201900014658-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2021149524-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9574075-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10435538-B2 |
priorityDate |
2009-12-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |