http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011150093-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_73ebc284a55d5daf0e209d6186c9e65c |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-12 |
filingDate | 2010-01-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a104fa1144c642e7f215441c7874405b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_67c0cae0d1e636e2a05a40665866c146 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5df48ecff8e15f18143be4b93452c8e3 |
publicationDate | 2011-08-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2011150093-A |
titleOfInvention | Liquid developer and method for producing liquid developer |
abstract | To provide a liquid developer excellent in dispersion stability of toner particles, and to provide a method for producing a liquid developer capable of easily producing such a liquid developer. A liquid developer according to the present invention includes an insulating liquid composed of a liquid containing a fatty acid component, and toner particles composed of a material containing a polyester resin and a fatty acid-modified alkyd resin. To do. The fatty acid-modified alkyd resin is preferably present in the vicinity of the surface of the toner particles. The oil length of the fatty acid-modified alkyd resin is preferably 40% or more and 90% or less. The liquid containing the fatty acid component is preferably a fatty acid ester. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012208383-A |
priorityDate | 2010-01-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 24.