http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011148940-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G4-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L79-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B17-56 |
filingDate | 2010-01-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9abb3e752a68859bb0d03422bb05c42d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5f99ecb41ec39639cef43fa2b7d2c5df http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f5ef296a4f7969c4df3ef6f1becb15ad |
publicationDate | 2011-08-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2011148940-A |
titleOfInvention | Biaxially stretched film |
abstract | A biaxially stretched film having excellent heat resistance and electrical insulation is provided. A biaxially stretched film using a thermoplastic polyetherketone resin as a main component and having a glass transition temperature (Tg) of 145 ° C. or higher and lower than 180 ° C., and having a glass transition temperature (Tg) of 180 ° C. or higher. The component is blended in an amount of 5 to 48% by mass. A biaxially stretched film having a dielectric breakdown voltage (BDV23) at 23 ° C. of 350 kV / mm or more. A biaxially stretched film having a ratio (BDV140 / BDV23) of a breakdown voltage (BDV140) at 140 ° C. to a breakdown voltage at 23 ° C. of 0.7 or more. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10221117-B2 |
priorityDate | 2010-01-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 28.