abstract |
PROBLEM TO BE SOLVED: To provide a resin composition having an excellent flame retardancy with a small amount of piperazine pyrophosphate added to a resin. [Solution] Piperazine pyrophosphate, melamine cyanurate, anti-drip agent and metal oxide are blended in a certain composition ratio to the resin. That is, 70 parts by mass of resin, 10-70 parts by mass of piperazine pyrophosphate (component A), 1-30 parts by mass of melamine cyanurate (component B), 0.01-1 part by mass of anti-drip agent (component C) and A flame retardant resin composition containing 0.1 to 4 parts by mass of a metal oxide (component D). [Selection figure] None |