http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011144247-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4af0df9a26ff4aafde7285cbd8eb12f4 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F265-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L55-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L69-00 |
filingDate | 2010-01-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_af2d0609cc21092abc99c6378271c382 |
publicationDate | 2011-07-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2011144247-A |
titleOfInvention | Polycarbonate resin composition and molded body |
abstract | Disclosed is a polycarbonate resin composition having excellent impact resistance. A resin (1) comprising a polycarbonate and an acrylonitrile-butadiene-styrene copolymer, and a polyfunctional monomer having two or more unsaturated bonds in the molecule is contained in an amount of 20% by mass or less. The first acrylic rubber component polymerized from the composition of No. 2 and the second composition containing 20% by mass or less of the polyfunctional monomer having two or more unsaturated bonds in the molecule, Composite rubber (A) 80 comprising a second acrylic rubber component having a glass transition temperature different from that of one acrylic rubber component, and 70% by mass or more and having a particle size of 0.3 μm or more and 0.7 μm or less in number distribution The vinyl monomer (B) is 0.1 mass% or more and 20 mass% or less (however, the total of the composite rubber (A) and the vinyl monomer (B) is 100 mass%. Grafted) And a graft copolymer (2). [Selection figure] None |
priorityDate | 2010-01-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |