http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011103297-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-50 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G75-23 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B1-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-02 |
filingDate | 2010-10-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5e608fc7d9b34563a4e17623e7204ea7 |
publicationDate | 2011-05-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2011103297-A |
titleOfInvention | POLYMER ELECTROLYTE AND METHOD FOR TREATING THE SAME |
abstract | A treatment method useful for evaluating the durability of a polymer electrolyte, which is simple and does not require a long-time fuel cell operation test, and can reproduce a state close to the operation state of a fuel cell. To provide a method for treating an electrolyte. The present invention relates to a method for treating a polymer electrolyte containing an ion exchange group, wherein water, iron ions and hydrogen peroxide are allowed to coexist in the polymer electrolyte, and then the water content of the polymer electrolyte is 20 wt. In this method, the polyelectrolyte is dried until it becomes less than or equal to%. The present invention also provides a first treatment in which the polymer electrolyte is immersed in an aqueous solution containing iron ions, and then the polymer electrolyte is dried until the water content based on the weight of the polymer electrolyte is 20% by weight or less. And a second treatment in which the polymer electrolyte that has undergone the treatment in the step and the first treatment step is dipped in hydrogen peroxide solution and then dried until the water content based on the weight of the polymer electrolyte is 20% by weight or less. And a processing method. [Selection] Figure 1 |
priorityDate | 2009-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |