http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011093279-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C33-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C59-02 |
filingDate | 2009-11-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_655719fd475cc36368f001a72eca85d4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cdb42d114c8041416c5599dec82c3437 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_314b7e38558ac4c0aef20902742c5b70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_751412465a46d22537909f552662abe8 |
publicationDate | 2011-05-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2011093279-A |
titleOfInvention | Method for producing mold for antiglare film and method for producing antiglare film |
abstract | Disclosed is a method for manufacturing a mold that can form irregularities on a mold surface in a desired shape with good accuracy and reproducibility, and is useful for manufacturing an antiglare film exhibiting high antiglare performance, and the method. The manufacturing method of the anti-glare film using the metal mold | die obtained by is provided. A step of applying a mirror finish to a surface 1 of a mold substrate 2, a step of forming a photosensitive resin film 3 on the mirror-finished surface, and exposing a pattern on the photosensitive resin film. The step of developing the photosensitive resin film 4 exposed with the pattern, the step of adjusting the surface shape of the photosensitive resin film by melting the developed photosensitive resin film, and the surface shape is adjusted. A process for forming a protective film 7 on the photosensitive resin film 6 produced, and a method for producing an antiglare film using the mold obtained by the method. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2017104831-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017111406-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10987884-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014117853-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013076899-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013176953-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013176954-A |
priorityDate | 2009-11-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |