http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011068958-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_adeb2a077d93bd496ec67fd5ab87cd0f |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C5-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F7-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F3-24 |
filingDate | 2009-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bd1c3e6848054e29523486ae335f1521 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3203be4cd5a399627baf170719972e05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f9405e88a0d5b704b353c19eb3615e5a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a2cfbc737d45374317a4456c2a4550d7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_97d467044c74924e0a17ab35404819d9 |
publicationDate | 2011-04-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2011068958-A |
titleOfInvention | Decorative metal article manufacturing method and decorative metal article |
abstract | The present invention provides a method for producing a decorative metal article and a decorative metal article obtained by combining a silver or silver alloy silver alloy sintering composition and a copper or copper alloy sintering composition. SOLUTION: One or more powders selected from copper and a copper alloy, containing 25 to 75% by weight of a first copper powder having an average particle size of 0.1 to 4.0 μm, and the balance having an average particle size of 4 A copper-containing plastic composition containing a mixed powder composed of a second copper powder having an average particle diameter of more than 0.0 μm and an average particle size of 10 μm or less and an organic binder, and one or more powders selected from silver and a silver alloy, A mixed powder and organic material containing 25 to 75 wt% of a first silver powder having a particle size of 0.1 to 4.0 μm, and the balance of the second silver powder having an average particle size exceeding 4.0 μm and an average particle size of 40 μm or less A copper-silver shaped body forming step for forming a decorative object by forming a combination with a silver-containing plastic composition containing a binder, and firing the obtained decorative object in the atmosphere at 660 to 770 ° C. for 3 to 40 minutes And a copper-silver shaped fired body production step for obtaining a fired fired article. [Selection] Figure 13 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104648028-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104648028-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013049874-A |
priorityDate | 2009-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 49.