classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G5-147 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G5-05 |
filingDate | 2009-07-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_031fc16ed471777a8c42dd92f8e3a054 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_18c911d49a33bfb0a212d1a6525c8e0e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f65b1c75272a660af441971cb18003cc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e66ccb10ea761c899419b37a8d8861f9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5581c7e0a52c8696f73bdb6da5508ad1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_03126fc2c2e3060819706b4a17c9ee77 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_67371f69028dc03ffd645dbd93c9d9f4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_675adef829dfd5bd6ab4343bada8f2e7 |
publicationDate | 2011-02-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2011027807-A |
titleOfInvention | Electrophotographic photosensitive member, image forming apparatus, and process cartridge |
abstract | An electrophotographic photosensitive member is provided which has a desired amount of initial wear and has improved wear resistance over time. An electrophotographic photoreceptor having a conductive substrate and a photosensitive layer containing fluororesin particles and metal oxide particles and having an outermost surface layer satisfying the following formulas (1) and (2): . Formula (1) 0.05 (μm / 1 reciprocation) ≦ Sa ≦ 0.2 (μm / 1 reciprocation) Formula (2) Sb / Sa ≦ 0.5 (In the above formulas (1) and (2), Sa Is less than 4 μm in depth from the surface in a test in which a sapphire needle with a radius of curvature of 0.1 mm at the tip is pressed against the outermost surface layer at a speed of 5 mm / s while being pressed with a load of 50 g and rubbed to a depth of 10 μm. (Sb represents the amount of wear per reciprocation in the region having a depth of 4 μm or more and 10 μm or less from the surface in the test.) [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10261430-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11112707-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016218212-A |
priorityDate | 2009-07-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 96.