http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011026365-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b19eaa8e535da4e4bceed99917a68153 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L79-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-12 |
filingDate | 2009-07-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_50731125efd0989610b49a8d59839c4c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6cffac95af02cd845308454246706f1f |
publicationDate | 2011-02-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2011026365-A |
titleOfInvention | Manufacturing method of resin molded body, resin molded body, optical component and optical device |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a resin molded body having a small variation in refractive index inside the resin molded body. The present invention also provides a resin molded body having small variations inside the resin molded body, and an optical component and an optical device excellent in performance using the resin molded body. The method for producing a resin molded body of the present invention comprises a resin composition comprising a resin having a refractive index of 1.6 or more, high refractive index particles having a refractive index higher than that of the resin, a dispersant, and a solvent. A method for producing a resin molded body, wherein a product is formed in a desired shape and is subjected to a first heating step and a second heating step of heating at a temperature higher than that of the first heating step, wherein a resin is formed in the first heating step. When the refractive index of the molded body is heated to the first refractive index (A1) and the resin molded body is heated to the second refractive index (A2) in the second heating step, the resin molding is performed. Heating is performed under such a condition that the difference in refractive index of the body (A2-A1) is 0.03 or more. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011079889-A |
priorityDate | 2009-07-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 301.