http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011021275-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2dcebf5a7f7ddc3b081f70e8ce1c4097
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-12993
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-24355
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C14-3414
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C14-185
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-0808
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C21-00
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F21S8-10
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C14-14
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C14-34
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F21V7-22
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F3-115
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C21-00
filingDate 2010-06-14-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a2ded779d80a38b80fbeeb1eae535713
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0471442c09ee3b8bb9c55f92358ca786
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_73418936790a48fcb96be17fe2aed0f7
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3d8bd378612a0e78b9395424499b1add
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f8f7572173d0bd54f9b388abb22f341a
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7bc5724c8789be6a4da0c571014608a9
publicationDate 2011-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber JP-2011021275-A
titleOfInvention Al alloy reflective film, reflective film laminate, automotive lamp, lighting fixture, and Al alloy sputtering target
abstract When a film is formed by sputtering, it has a higher reflectance than a pure Al film, and has excellent alkali resistance, acid resistance, and moisture resistance, which causes a decrease in reflectance even without a protective film. A difficult Al alloy reflective film, a reflective film laminate having such an Al alloy reflective film, an automotive lamp, a lighting fixture, and an Al alloy sputtering target capable of forming such an Al alloy reflective film are provided. To do. (1) One or more elements of Sc, Y, La, Gd, Tb, and Lu are contained in a total amount of 0.4 to 2.5 at%, and the balance is made of Al and unavoidable impurities, Al alloy reflective film characterized in that the roughness of the film surface measured with a force microscope is 4 nm or less, (2) Automotive lamps and lighting equipment having this reflective film, (3) Al alloy sputtering target for forming. [Selection] Figure 3
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2017134879-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013253278-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20180097697-A
priorityDate 2009-06-15-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006091698-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H07301705-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001028348-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H10195651-A
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419544299
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID13830

Total number of triples: 35.