Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1664ce18a172f84c0bd96e3e3a6cdb86 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61J1-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61J1-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-521 |
filingDate |
2009-07-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9fc8775242a3f4fc0300c0a6c433125f |
publicationDate |
2011-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2011021048-A |
titleOfInvention |
Chemical liquid filling container and chemical liquid filling preparation using the same |
abstract |
Disclosed is a chemical solution filling container which contains a nucleating agent to be added to an ethylene-propylene copolymer at an optimum ratio and is excellent in hygiene, heat resistance, transparency and pressure resistance. A chemical solution filling container according to the present invention comprises 0.15 to 0.20 weight per 100 weight parts of (A) ethylene-propylene copolymer resin containing 0.5% to 1.2% ethylene content. Part (B) of a cyclic organophosphate metal salt and 0.04 to 0.06 parts by weight of (C) calcium stearate are obtained by molding a polyolefin resin composition. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2013168717-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2013168717-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10577483-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016051989-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20150013760-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102071437-B1 |
priorityDate |
2009-07-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |