http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010526922-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-523 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-41 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-103 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-005 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L69-005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F279-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L51-003 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F253-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F279-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L55-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-521 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-12 |
filingDate | 2008-05-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2010-08-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010526922-A |
titleOfInvention | Impact-resistant polycarbonate composition |
abstract | The present invention relates to (A) aromatic polycarbonate and / or aromatic polyester carbonate, 10 to 99 parts by weight, (B) (B.1) B.I. 2 at least one vinyl monomer, 5 to 95 wt. %, (B.2) one or more graft bases having a glass transition temperature of less than 10 ° C., 95-5 wt. % Rubber-modified graft polymer, 1 to 35 parts by weight, (C) vinyl (co) polymer and / or polyalkylene terephthalate excluding copolymer of α-methylstyrene and acrylonitrile, 0 to 40 parts by weight, (D) phosphorus A composition containing 0 to 50 parts by weight of the flameproofing agent, 0 to 50 parts by weight based on the sum of components A + B + C, and (E) 0 to 50 parts by weight based on the sum of components A + B + C. Formula (I) Component B. using an emulsifier of 1 and graft base It is obtained by reaction by emulsion polymerization with 2, and relates to a composition excellent in high hydrolysis resistance. The invention further relates to the use of this polycarbonate composition in the manufacture of molded articles and to the molded articles themselves. |