http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010525121-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-139 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F10-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-18 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-654 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F210-08 |
filingDate | 2008-04-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2010-07-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010525121-A |
titleOfInvention | Butene-1 terpolymer and process for producing the same |
abstract | Propylene derived units content of 0.5 to 13 mol%; and content of 3 mol% ethylene derived units; 1-10, the ratio of the content of propylene derived units and the ethylene derived units C 3 / C 2; With a melt flow rate MIE of 0.3-3 g / 10 min measured at 190 ° C./2.16 kg, and a Mw / Mn ratio of 4-10 measured by GPC, 1 × 10 A butene-1 terpolymer having a molecular weight distribution curve with a molecular weight portion of 5 or less accounting for 22% or more of the total area. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014500340-A |
priorityDate | 2007-04-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 53.