http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010270298-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_efbfdc7316d3b1b7ceaee5366a61b6e0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F112-12 |
filingDate | 2010-01-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_774a10997de894de7b61b6db55cbd725 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_de8ac524269d38385b9c3124ff217be8 |
publicationDate | 2010-12-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010270298-A |
titleOfInvention | Rubber composition and tire using the same |
abstract | To provide a rubber composition exhibiting excellent dry grip performance in a wide temperature range from a low temperature range to a high temperature range. The rubber composition of the present invention is obtained by polymerizing a styrene monomer represented by the formula (I) with respect to 100 parts by mass of a rubber component composed of at least one diene polymer, and has a weight average molecular weight ( Mw) is blended in an amount of 1 to 100 parts by mass of a resin having a Mw of 4,000 to 40,000. [Selection figure] None |