Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_95585944cd76ddfb6dc33ed2a0b84403 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-6592 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F210-06 |
filingDate |
2010-07-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c418f3e0892b8af043eb60811530b25e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ab7fec74c31e1c01a74101820fbcb387 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b0adfd5205e5f414c5b665baeaae32d2 |
publicationDate |
2010-11-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2010265473-A |
titleOfInvention |
PROPYLENE COPOLYMER, RESIN COMPOSITION COMPRISING THE COPOLYMER, AND MOLDED BODY |
abstract |
To provide a propylene-based polymer which gives a molded product with less stickiness and excellent flexibility and transparency. A propylene polymer satisfying the following (1) and (2). (1) The amount of components eluted in hexane at 25 ° C. is 0 to 80% by mass. Satisfies the relationship of (Tm-140) [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2017164410-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015005374-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020037660-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2018164161-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108884283-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020050226-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7311955-B2 |
priorityDate |
1999-03-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |