Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_73ebc284a55d5daf0e209d6186c9e65c |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L41-39 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L41-083 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L41-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-462 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L41-187 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L41-333 |
filingDate |
2009-05-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f3b304033b699ba0b734b4afab17a5f6 |
publicationDate |
2010-11-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2010265146-A |
titleOfInvention |
Ceramic manufacturing method, ceramics, piezoelectric actuator, liquid ejecting head, and liquid ejecting apparatus |
abstract |
An object of the present invention is to provide a method for producing ceramics in which the environmental load is reduced by using a specific binder. A method for producing a ceramic includes obtaining a barium titanate dispersion containing at least one selected from an alginate, an alginic acid derivative and agar, barium titanate particles, and water, and the titanic acid. The method includes forming a barium dispersion into a desired shape to obtain a barium titanate molded body, and heat-treating the barium titanate molded body. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11647677-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012126636-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7348751-B2 |
priorityDate |
2009-05-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |