Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3e331bcae33f8cd58d8b1eb6e5c117ca |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-548 |
filingDate |
2009-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4ca9b47eca5e61e3501dc39106bc9195 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_84de03b05d1bcfc26597c96e67dac394 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_df8052e4bd04eed0a51620f387110dd9 |
publicationDate |
2010-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2010235906-A |
titleOfInvention |
Fluoro rubber composition and rubber molded product using the same |
abstract |
[PROBLEMS] To provide a fluororubber that is less likely to break even when used under high temperature and high compression in a fluororubber composition used in a rubber molded product such as an O-ring. [Solution] By setting the crosslink density of the fluororubber to 1.0 × 10 −3 mole / cc or less, it is possible to obtain a fluororubber that does not easily break even under high temperature and high compression. By adding mercaptosilane to this, compression set can be kept low, and by adding diatomaceous earth in addition to this, a fluororubber composition having excellent adhesion to metal can be provided. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113681740-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20200059225-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20220158012-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019070040-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11767410-B2 |
priorityDate |
2009-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |