Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6c8d4dc7bd1a30d8fda907fceaeb4e69 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2067-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C45-1816 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-183 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C45-0001 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-183 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-00 |
filingDate |
2010-07-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b98b1b922ae0098ccaac331dd51c6cf9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9f51fea86ea78771210c6aaec88c115d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8a1c2f814ab70e285d79970937a039f4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6a8873276666038d3c3f15a5aa94015c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8c6fcba8ebb7ee4f7d213c7938219efe |
publicationDate |
2010-10-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2010229419-A |
titleOfInvention |
Method for producing polyethylene terephthalate resin and polyester resin molding |
abstract |
Disclosed is a polyethylene terephthalate resin in which the amount of acetaldehyde by-product during melt molding is small and the acetaldehyde content in a molded body is reduced. An intrinsic viscosity [η 2 ] is 0.70 dl / g or more and 1.50 dl / g or less, an acetaldehyde content [AA 0 (weight ppm)] is 10 weight ppm or less, and a water content is 30 ± 20. The acetaldehyde content [AA 1 (wt ppm)] of the molded product obtained by adjusting the weight to ppm by weight and injection molding at 280 ° C. and the moisture content were adjusted to 120 ± 20 wt ppm and injected at 280 ° C. Polyethylene terephthalate resin in which the acetaldehyde content [AA 2 (weight ppm)] of the molded product obtained by molding satisfies the following formula (1). [Expression 1] [Selection figure] None |
priorityDate |
2003-11-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |