http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010229191-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_27aa3092499b93e3144b5053272698ca |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03B21-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L69-00 |
filingDate | 2009-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0f13bc0ecb76563e73676fb5822d5a17 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f6e5aaac076a36f161b273d698d47333 |
publicationDate | 2010-10-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010229191-A |
titleOfInvention | Aromatic polycarbonate resin composition and molded article |
abstract | An aromatic polycarbonate composition excellent in appearance, flame retardancy and light reflectivity, and a resin molded product thereof are provided. SOLUTION: To 100 parts by mass of an aromatic polycarbonate resin (A), 11 to 23 parts by mass of a titanium oxide-based additive (B) containing alumina and silicon compounds, 0.01 to 1 of polyfluoroethylene (C) .5 parts by mass, the Al 2 O 3 content a (mass%) of the titanium oxide additive (B), the SiO 2 content s (mass%) in the titanium oxide additive, and titanium oxide When the average particle diameter (μm) is d, (Formula 1) 125 ≧ (s / d 2 )> (a / d 2 ) An aromatic polycarbonate resin composition characterized by satisfying [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021193221-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011032447-A |
priorityDate | 2009-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 193.