http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010202675-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c06ff00cc23d0d0c48233a171dccb984 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-00 |
filingDate | 2009-02-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_31cd62f8520fab3dd6da77cf793b02aa http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0af50f0fd7f8f8458a9445f9ba565e52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_01738a784f7387cc04d441d0512e9244 |
publicationDate | 2010-09-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010202675-A |
titleOfInvention | Film for printing |
abstract | Provided is a resin film for printing which is excellent in solvent resistance and can be printed directly, and has excellent characteristics such as heat resistance and moisture absorption resistance. SOLUTION: A thickness of 50 to 75 obtained by molding a thermoplastic resin composition (I) comprising (A) 25 to 75% by mass of a rubber-modified styrene resin and (B) 25 to 75% by mass of a polyamide resin. A 500 μm printing film is provided. The component (A) is a graft copolymer obtained by polymerizing a vinyl monomer in the presence of a rubbery polymer, or a (co) polymer of the graft copolymer and a vinyl monomer. And a mixture. In addition to the aromatic vinyl compound and the vinyl cyanide compound, the vinyl monomer contains 0.1 to 1.2% by mass of the functional group-containing vinyl monomer in the component (A), and the component (A) The intrinsic viscosity of acetone (methyl ethyl ketone, 30 ° C.) is 0.15 to 1.5 dl / g. 5-30 mass parts rubbery polymer is contained with respect to 100 mass parts of composition (I). [Selection figure] None |
priorityDate | 2008-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 169.