http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010191218-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c5520dd38cc403678d9f91e0b0ee95fb |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-08 |
filingDate | 2009-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e15499abfef705d3e63e2c5f292e7dd5 |
publicationDate | 2010-09-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010191218-A |
titleOfInvention | toner |
abstract | PROBLEM TO BE SOLVED: To provide a toner capable of shortening the warm-up time by improving the low-temperature fixability without impairing the high-temperature offset resistance. A toner contains a binder resin, a colorant and a wax. The binder resin contained in such a toner includes a cross-linked styrene acrylic resin. The crosslinkable styrene acrylic resin includes a carboxyl group-containing styrene acrylic resin, a glycidyl group-containing styrene acrylic resin, and a crosslinking component that crosslinks the carboxyl group-containing styrene acrylic resin and the glycidyl group-containing styrene acrylic resin. The crosslinking component is 5% by weight or more and 40% by weight or less based on the total amount of the binder resin. The acid value of the cross-linked styrene acrylic resin is 3 KOHmg / g or more and 25 KOHmg / g or less. The wax includes paraffin wax and ester wax. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018205706-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7091134-B2 |
priorityDate | 2009-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 146.