http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010170908-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9d5ebd9bdc11f7a4b267d7e865d5a84f |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M2-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M6-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-06 |
filingDate | 2009-01-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ae6a6f7a8c815fbdf2b2c9f835f6275e |
publicationDate | 2010-08-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010170908-A |
titleOfInvention | Manufacturing method of flat primary battery and flat primary battery |
abstract | An object of the present invention is to provide a method for manufacturing a flat primary battery and a flat primary battery which are inexpensive and have a good battery capacity. In a method of manufacturing a flat primary battery 1 in which a positive electrode mixture 5 is accommodated in a positive electrode can 2, a positive electrode mixture 5 containing nickel oxyhydroxide and silver oxide is accommodated in the positive electrode can 2, and the positive electrode can 2, nickel oxyhydroxide and silver oxide are reacted to form a silver / nickel composite oxide, and the mass ratio of nickel oxyhydroxide is 0.61 or more, 1.0 with respect to silver oxide. The following. [Selection] Figure 1 |