http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010159358-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1af8df51ce24ca931ae718fb747f6aa0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-34 |
filingDate | 2009-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fb93a323aff9410a267a3867d6efac79 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3d5b1aed1889ca7dd92988025ba82d32 |
publicationDate | 2010-07-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010159358-A |
titleOfInvention | Method for producing polymer having sulfonic acid group and amide group |
abstract | An object of the present invention is to provide a method for reducing the amount of phenol generated as a decomposition product of triphenyl phosphite used as a condensing agent in producing a polymer having a sulfonic acid group and an amide group. The following chemical formula (1) A method for producing a polymer comprising a unit represented by A polymer containing a unit represented by the following chemical formula (2); A polymer containing a unit represented by the following chemical formula (3) In combination with at least one amine compound containing a sulfonic acid group represented by the above, triphenyl phosphite and phosphorous acid triester (the ester is selected from methyl, ethyl, propyl) as a condensing agent used. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114107655-A |
priorityDate | 2009-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 168.