http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010155945-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_758994071efb42b565fc2c04637be131 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D157-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D167-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J175-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J167-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J201-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D201-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 |
filingDate | 2008-12-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f325793f4e73e41c32d808a5e6b3352b |
publicationDate | 2010-07-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010155945-A |
titleOfInvention | Resin particles and method for producing the same |
abstract | PROBLEM TO BE SOLVED: To find a production method for easily obtaining resin particles having irregularities on the surface. An organic solvent (u) solution (O) of an aqueous dispersion (W) of resin particles (A) containing a resin (a) and a precursor (b0) of the resin (b) and / or (b). ), (O) is dispersed in (W), and (b0) is further reacted as necessary to form resin particles (B) containing (b) in (W), A method for producing (C), wherein an aqueous dispersion (X) of resin particles (C) having (A) attached to the surface of (B) is obtained, and (u) and water are further removed from (X), (O) contains the poor solvent (u1) and the good solvent (u2) of (b), and utilizes the difference in boiling point or solubility in water after the formation of (B) (u1) and (u2), (B) to (u2) alone is desolvated, (u1) and (b) are phase-separated in (B), and (u1) is desolvated from (B), as well as ( A method for producing resin particles in which the shape factor (SF-2) of C) is 110 to 300. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012058489-A |
priorityDate | 2008-12-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 795.