http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010150718-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4a60326471cf8e73187625e940919ea0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H19-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H27-20 |
filingDate | 2008-12-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c45b34ce44575cc31c55f20428fea82c |
publicationDate | 2010-07-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010150718-A |
titleOfInvention | Processing paper |
abstract | To provide a processed paper that is particularly excellent in dimensional stability and releasability. The base paper comprises at least a base paper and a coating layer, and the base paper is a color table by a C dyeing method in accordance with a paper, paperboard and pulp-fiber composition test method specified in JIS-P8120 (1998). The blending ratio of the mechanical pulp measured based on the above is 40 to 70%, an inorganic pigment is internally added, and the ash content measured according to JIS-P8251 (2003) is 10 to 30%, The coating layer is formed by applying a coating solution containing a water-soluble resin to at least one surface of the base paper, and tetrabromophenolphthalein ethyl ester potassium salt described in Papier 28.101 (1974). It is colored blue in a color test using (TBP). [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105091754-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019077957-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7073073-B2 |
priorityDate | 2008-12-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 180.