http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010150638-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5198a2a21392d6cbc0bb4898b3fb3d29 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P10-20 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C21C7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C21C7-076 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C21C5-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B5-06 |
filingDate | 2008-12-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2d8ca20b7f059945cc9c5af025171f3c |
publicationDate | 2010-07-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010150638-A |
titleOfInvention | Slag regulator |
abstract | To provide a slag adjusting agent having a high dissolution rate in slag and good handleability. The slag adjusting agent is mainly composed of 20% by mass or more and 98% by mass or less of MgO in terms of oxide, with the balance being at least one of CaO, SiO 2 , calcium carbonate, and calcium hydroxide. A raw material composed of one or more kinds and inevitable impurities, 0.1% by mass or more and 2.0% by mass or less of a foaming agent by outer coating, and 0.01% by mass or more and 0.2% by mass by outer coating. At least one of the following organic fibers is added, and a binder is further added to knead, mold, and dry. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012158495-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113913583-A |
priorityDate | 2008-12-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 39.