Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_eece3f4c4266dfce4fc469ddcb3eb4e9 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-24 |
filingDate |
2008-11-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ea66ef521d86cc946e88e10d7ccf2844 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7c31dc056b19800323a30103d57f8067 |
publicationDate |
2010-06-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2010126645-A |
titleOfInvention |
Epoxy resin composition |
abstract |
Provided is an epoxy resin composition having a low dielectric constant of a cured product obtained with excellent adhesion. An epoxy resin containing 50 to 90 wt% of an epoxy resin 1 represented by the following formula (1) and 100 parts by mass of an epoxy resin 2 containing 10 to 50 wt% of an epoxy resin 2 represented by the following formula (2). An epoxy resin composition containing 20 to 200 parts by mass of a modified cyclic olefin polymer having a group and / or an acid anhydride group. (In formula (1), n is 1-10.) [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7198775-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010185034-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2019123934-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019123934-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015529266-A |
priorityDate |
2008-11-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |