http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010110898-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 |
filingDate | 2008-11-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_450fa2de380cb61d24aecd90453a582d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f3fb799fb27e6cffbe4791a6f3401e02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2834ee240e8610258e28fbc50ca61047 |
publicationDate | 2010-05-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010110898-A |
titleOfInvention | Thermal laminated laminated film and method for producing the same |
abstract | To provide a PPS heat laminated laminated film having excellent moldability and carbon dioxide gas refrigerant resistance. A laminated film having a structure in which a biaxially oriented polyarylene sulfide film and a biaxially oriented copolymerized polyarylene sulfide film are thermally laminated without an adhesive layer, wherein the thermally laminated laminated film is A heat laminated laminate film having a room temperature breaking elongation of 80% or more and 160% or less and 100 bubbles or less of 5 mm or more per 1 m 2 of the heat laminated laminate film after the carbon dioxide gas refrigerant cycle test. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7268346-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012155854-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019116092-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013006377-A |
priorityDate | 2008-11-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 112.