http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010102893-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_50ff960bba3c8cfabd7f3141e0ff0189 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H27-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H13-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B3-52 |
filingDate | 2008-10-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8cefaa21507658b1841c670139ceeed0 |
publicationDate | 2010-05-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010102893-A |
titleOfInvention | Meta type wholly aromatic polyamide electrical insulation paper |
abstract | The present invention provides a meta-type wholly aromatic polyamide electrical insulating paper that has excellent flame retardancy while suppressing gas generation during high-temperature processing, and has an excellent balance between breaking strength and dimensional stability in a high-temperature atmosphere. To do. SOLUTION: A porous coagulated yarn is obtained by wet spinning using a specific coagulation bath, followed by plastic stretching at a specific magnification, and further by performing a specific heat treatment in saturated steam. The residual solvent amount remaining in the fiber is 1.0% by mass or less, the dry heat shrinkage at 300 ° C. is 3.0% or less, and the breaking strength is 3.0 cN / dtex or more. A short fiber of type wholly aromatic polyamide fiber is used. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102201806-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20180022751-A |
priorityDate | 2008-10-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |