http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010100823-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a696e8ab693ab78a931db09817fad566 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-18 |
filingDate | 2009-07-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a30ce36ab2fa4b860252beb9151cce94 |
publicationDate | 2010-05-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010100823-A |
titleOfInvention | Expandable styrene resin particles |
abstract | 【Task】 There is no blocking during pre-foaming, the foamed particles are excellent in fluidity, the peeling of the coated drug is suppressed, the fusion is good, and no oil leaks. [Solution] Expandable styrene resin particles obtained by impregnating a styrene resin particle with a foaming agent, and the expandable styrene resin particles have the resin particle surface coated with a composition, The composition comprises polyethylene glycol A having a molecular weight of less than 400 covering the resin particle surface, 0.003 to 0.04 parts by weight of fatty acid amide or fatty acid bisamide with respect to 100 parts by weight of the resin particles, Consisting of 0.2 to 0.8 parts by weight of a fatty acid metal salt and 100 parts by weight of resin particles and polyethylene glycol B having a molecular weight of less than 400; The polyethylene glycols A and B are contained in 0.02 to 0.08 parts by weight with respect to 100 parts by weight of the resin particles, and are coated in two portions. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012236224-A |
priorityDate | 2008-09-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 120.