Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_758994071efb42b565fc2c04637be131 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-85 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-08 |
filingDate |
2008-10-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a7aad16f1580b25f006735ea71f925a6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_240b1155ceed6a7ccfcefcb051c8d7de |
publicationDate |
2010-04-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2010096928-A |
titleOfInvention |
Resin for toner and toner composition |
abstract |
PROBLEM TO BE SOLVED: To develop a resin for toner that has both hot offset resistance and low-temperature fixability even in the use of toner with high speed and energy saving. SOLUTION: The THF-insoluble content is 3 to 45% by weight, the peak-top molecular weight of gel permeation chromatography of the THF-soluble content is 3500 to 25000, the softening point is 120 to 185 ° C., and the titanium element is 20 to 2000 ppm. And a non-linear polyester resin (A) containing 10 to 1200 ppm of a nitrogen element. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015143854-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11281117-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013033176-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014016551-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015135487-A |
priorityDate |
2008-10-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |