http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010091850-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1af8df51ce24ca931ae718fb747f6aa0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G5-147 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G5-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G5-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G21-00 |
filingDate | 2008-10-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_82ef06fc3746749a627f3fc3a68f80cb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5215e773b23d931caed628625a650ed0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_395aa7f5973926d009d8ce5c3d4fe8a5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e7a4eec02cca2c889232529a9b4209a1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7f656619d0471c62960453b514b26deb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ef723e9feec1bc67bd192f81ab3a7208 |
publicationDate | 2010-04-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010091850-A |
titleOfInvention | Image forming method |
abstract | An image forming method that prevents / suppresses image flow is provided. A surface layer of a photoreceptor is polymerized and cured by heat, light and radiation of a hole transporting compound having a (meth) acryloyloxy group, an internal reflection element is Ge, an incident angle is 45 degrees, and a Fourier transform. A value of the formula (1) obtained by infrared spectroscopic total reflection method is 0.019 or more and 0.040 or less, A = S1 / S2 (1) (S1 is the peak area of terminal olefin (CH 2 =) in-plane bending vibration. S2 is the peak area of C = O stretching vibration of (meth) acryloyloxy group.) The ten-point average roughness of the surface of the photoreceptor is 0.2 μm ≦ Rz ≦ 0.8 μm, The 10-point square 10-point average surface roughness of the surface of the photoreceptor is 60 nm or more and 200 nm or less, The cleaning step is a step of rubbing the surface of the photoconductor through abrasive particles made of inorganic fine powder of a perovskite type crystal having an average particle size of 80 nm or more and 220 nm or less and having an approximately cubic or rectangular parallelepiped shape. Method. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019152699-A |
priorityDate | 2008-10-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |