Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4a60326471cf8e73187625e940919ea0 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H21-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A47K10-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H21-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H27-00 |
filingDate |
2008-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d1b4ab0525f0d5bc76150d8e3775809a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b148e1c781acae2732f05fdd44dac240 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a7d67b88f24ed1702eea19334c86fecf |
publicationDate |
2010-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2010084283-A |
titleOfInvention |
Paper towel and paper towel manufacturing method |
abstract |
[Problem] To provide a paper towel excellent in strength and waist and a method for producing the same while maintaining the previous paper thickness by adding a softener while suppressing the amount of pulp used. A paper towel having a basis weight of 34 to 45 g / m 2 , a paper thickness of 140 to 190 μm, and a softening agent added at a rate of 0.5 to 10.0 kg / t as a bulking agent, excellent in strength and waist In order to obtain a paper towel, a dry paper strength enhancer was internally added at a rate of 2.0 to 20.0 kg / t. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102055430-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012180609-A |
priorityDate |
2008-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |