http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010082849-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d93502a23a72b56472bc75854cfe7c60 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K45-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C33-40 |
filingDate | 2008-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_51359f4eba220a315c82f832fb292ce5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_60c3d158784caf564c5b8c09fba96fd7 |
publicationDate | 2010-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010082849-A |
titleOfInvention | RESIN COMPOSITION, RESIN MOLD, AND METHOD FOR PRODUCING MOLDED BODY USING THE RESIN MOLD |
abstract | [PROBLEMS] To provide a resin composition having good releasability from a mold during molding and stringing property, a resin mold having excellent releasability, and a method for producing a molded body using the resin mold. A shear rate of a resin composition containing an alicyclic structure-containing thermoplastic resin and a resin composition containing 0.02 to 0.20 parts by mass of a hydroxyl group-containing ester compound with respect to 100 parts by mass of the resin composition. The shear viscosity at 10,000 / s is 20 to 50 Pa · s, and the extension viscosity at 230 ° C. and the extension rate 100 / s is 6 to 20 kPa · s. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015160399-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102076376-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20140142228-A |
priorityDate | 2008-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 152.