http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010037141-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fec576c38e34882531ca37d6b922bf42 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D201-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01F5-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 |
filingDate | 2008-08-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7cbeeb5962b437e30782d13b1e81c9bb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f5756ce578a75ac28c015ee3fb25cebe http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_540ddd3c5ccdf4fb5ad29a087d7d1a3b |
publicationDate | 2010-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010037141-A |
titleOfInvention | Flaky substances and coating compositions |
abstract | The present invention provides a flaky material capable of suppressing the visible light reflectivity of an article by making the flaky material a structure formed of a material having a small visible light reflectivity itself. This is the issue. The flaky material of the present invention is a flaky material comprising an aggregate of fine particles, and the aggregate is formed by consolidating the fine particles and the fine particles, and the fine particles are magnesium fluoride. It is characterized by containing. Preferably, the fluorinated magnesium is MgF 2-x (OH) x (x = 1 to 0). Furthermore, the average particle diameter of the fine particles is preferably 5 to 100 nm. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012076967-A |
priorityDate | 2008-08-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 75.