http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010032590-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_669c01133740c5233f2c8738904ea3af |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-13363 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1339 |
filingDate | 2008-07-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c7046e6633f598a4dec4488e2721424b |
publicationDate | 2010-02-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010032590-A |
titleOfInvention | Optical element manufacturing method, optical element, and liquid crystal display device including the optical element |
abstract | The present invention provides a manufacturing method for manufacturing an optical element including a retardation layer in which surface unevenness is suppressed. In a method for manufacturing an optical element 1 having a base material 2, a retardation layer 3 obtained by polymerizing a liquid crystal composition, a transparent conductive film 5, and a columnar body 4, the substrate 2 is directly applied. Or indirectly, a liquid crystal composition containing a polymerizable liquid crystal compound is applied to produce a liquid crystal coating film, and the polymerizable liquid crystal compound contained in the liquid crystal coating film is polymerized to form the liquid crystal coating film as the retardation layer 3. A phase difference layer forming step, a transparent conductive film forming step of forming a transparent conductive film 5 with a conductive film composition containing a conductive material directly or indirectly with respect to the base material 2; And a columnar body forming step of forming a columnar body 4 by directly or indirectly applying and polymerizing a resin composition containing a photocurable resin, and the retardation layer forming step and the columnar body forming step were performed. Later, by performing a transparent conductive film forming step, the surface unevenness is suppressed. Optical element 1 having a phase difference layer that is is provided. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101916976-B1 |
priorityDate | 2008-07-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 111.