http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010013590-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e2b60c751b9b6855cd19a5127595779f |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61F13-49 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F10-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61F13-15 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61F13-514 |
filingDate | 2008-07-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_49438c68be4caa0180f820bf8e7f4b84 |
publicationDate | 2010-01-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010013590-A |
titleOfInvention | Polyethylene resin composition and sanitary article backsheet using the same |
abstract | An object of the present invention is to improve the tensile strength and elongation characteristics of a hygiene product back sheet to improve the easy peelability of the back sheet from underwear after use, and also improve the molding processability. A polyethylene resin composition useful as a sheet material is developed. A linear low density polyethylene resin (A) having a density of 0.880 to 0.930 g / cm 3 and having a minimum differential value (dN / dS) of an elongation load curve in a tensile test greater than 0. ) 10 to 40% by weight of a branched low density polyethylene resin (B) having an MFR (190 ° C., 21.18 N load) of less than 6 g / 10 minutes and an MFR of 6 g / 10 minutes or more. A polyethylene-based resin composition comprising 3 to 20% by weight of a branched low-density polyethylene-based resin (C). [Selection] Figure 2 |