http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010001401-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0ddb9f3656270bc5410be3679322fead |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G65-38 |
filingDate | 2008-06-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8aed10cd264135ee7481cbe1743f5ee9 |
publicationDate | 2010-01-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010001401-A |
titleOfInvention | Method for producing low molecular weight poly (2,6-diarylphenylene ether) |
abstract | PROBLEM TO BE SOLVED: To provide a method for efficiently producing low molecular weight poly (2,6-diarylphenylene ether). SOLUTION: A production method in which a phenol derivative is polymerized in a mixed solvent of an aliphatic alcohol and a ketone or ether organic solvent in the presence of a catalyst and oxygen to precipitate a polymer, and the composition of the mixed solvent And / or producing a poly (2,6-diarylphenylene ether), wherein polymers having different molecular weights are precipitated by changing the mixing ratio. The ketone-based or ether-based organic solvent is preferably contained in a proportion of 5 to 60% by weight with respect to the aliphatic alcohol. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5730894-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105095214-A |
priorityDate | 2008-06-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 49.