http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010001390-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L45-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-189 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L65-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 |
filingDate | 2008-06-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dc26548af70a21fbd2afdc53acb0039d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c488fe0f552895a6c90507bb9e356758 |
publicationDate | 2010-01-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010001390-A |
titleOfInvention | Biaxially oriented film |
abstract | The present invention provides a biaxially oriented film that has both high dimensional stability against changes in humidity and dimensional stability during processing at high temperatures after making the product. The polycycloolefin (b) has a glass transition temperature in the range of 110 to 180 ° C., and the polyester (a) and the polycycloolefin (b). A biaxially oriented film having at least one film layer in which the weight ratio of olefin (b) is in the range of 97: 3 to 60:40. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4688311-A |
priorityDate | 2008-06-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 56.