abstract |
The water-swellable linear polymer is obtained by reacting together polyethylene oxide having a number average molecular weight of less than 4000, an aliphatic diol, and a difunctional isocyanate. The controlled release composition consists of the linear polymer and an active agent. The polymer can carry a pharmaceutically active agent with a molecular weight of 200-20,000. |