Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-24413 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K9-06 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82B3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-1618 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D201-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D1-02 |
filingDate |
2007-05-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2009-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2009541544-A |
titleOfInvention |
Antifouling coating containing nanoscale hydrophobic particles and method for producing the same |
abstract |
An antifouling coating comprising a resin binder layer containing nanoscale hydrophobic particles, wherein the particles are not only located in the binder layer but also protrude from the layer, the particle / binder The ratio is 2.5-5 and the concentration of the particles in the binder layer is 0.01-1 g / m 2 . |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101887075-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014062215-A |
priorityDate |
2006-06-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |