Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2229-37 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2229-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C2529-40 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C2-66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J29-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C2-68 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J29-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J29-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J29-06 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07B61-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C2-86 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B39-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C15-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J29-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-04 |
filingDate |
2006-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2009-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2009521318-A |
titleOfInvention |
Bound phosphorus-modified zeolite catalyst, its preparation and use |
abstract |
A bound phosphorus modified zeolite catalyst is disclosed. The zeolite is treated with a phosphorus compound to form a phosphorus-treated zeolite. The binder material is treated with mineral acid before being combined with the phosphorus-modified zeolite. Binder materials include inorganic oxide materials such as alumina, clay, aluminum phosphate and silica-alumina, especially binders of alumina or clay or combinations thereof. Mineral acids include hydrochloric acid, nitric acid, phosphoric acid or sulfuric acid. The phosphorus-treated zeolite is combined with an acid-treated inorganic oxide binder material to form a zeolite-binder mixture. Water is added to form an extrudable paste that can be formed and heated to a temperature of about 4000 ° C. or higher to form a bound phosphorus-modified zeolite catalyst. For aromatic alkylation, the bound phosphorus-modified zeolite catalyst is contacted with an alkylating agent and an aromatic alkylation feed of an aromatic compound under reaction conditions suitable for aromatic alkylation. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013512964-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013517319-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017114755-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8981173-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015513459-A |
priorityDate |
2005-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |