http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009300733-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_be92719b856db86c092cc233e9512ca2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-08 |
filingDate | 2008-06-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_65d807b830b92b7ab9d7a9774afce16c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d2490e16bfcfdc04cbe6cc0e69c9a2dc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bdba489033e5c1e0a78c9b8d9db7245a |
publicationDate | 2009-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009300733-A |
titleOfInvention | Manufacturing method of toner for developing electrostatic image, toner, image forming apparatus, and process cartridge |
abstract | A toner manufacturing method that has no cleaning between character portions and does not deteriorate fine line reproducibility and that can be easily cleaned, and toner, and an image forming apparatus using the toner, And providing a process cartridge. A toner composition containing at least a resin, a colorant, and a release agent is dissolved or dispersed in an organic solvent, the dissolved or dispersed material is used as an oil phase dispersion, and the oil phase dispersion is used as a fine particle dispersant. Disperse in an existing aqueous medium, and supply the resulting emulsified dispersion to a continuous vacuum defoamer and thin the film by centrifugal force, thereby applying an organic solvent while applying a shearing force to the emulsified dispersion. A method for producing a toner for developing an electrostatic charge image, which is removed to form a toner base, wherein the oil phase dispersion contains a layered inorganic mineral in which at least some of the ions between layers are modified with organic ions, and the oil phase The thixotropy value (TI value) of the dispersion is adjusted to 1.3-5. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8507164-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8535864-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8563205-B2 |
priorityDate | 2008-06-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 229.