http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009282173-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_758994071efb42b565fc2c04637be131 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 |
filingDate | 2008-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2740c677f63139c6badd6f5b8fc26726 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e0815e26dd8ee3f283148c4d91ecd484 |
publicationDate | 2009-12-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009282173-A |
titleOfInvention | Method for producing resin particles for toner |
abstract | An object of the present invention is to provide a method for producing resin particles for a toner excellent in both storage stability and low-temperature fixability. [Solution] Sol-gel method, specifically, solvent (S) containing no active hydrogen, preferably 5 to 20 carbon atoms Metal alkoxide (d), preferably silicon or aluminum alkoxide, in contact with the surface of the resin particles (A) having at least one of a hydroxyl group and a carboxyl group on the surface. The resin particles for toner are produced by the method for producing resin particles for toner, wherein the layer (B) of the product (c) is formed. [Selection figure] None |
priorityDate | 2008-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |