Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1af8df51ce24ca931ae718fb747f6aa0 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41J2-17513 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H1-4291 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H1-541 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41J2-175 |
filingDate |
2008-05-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a2eaad68df4272f07854af1ae844999f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_02d44223f334f724d7b754079549eee2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_572d06c9114606a9352fc8e11da0414c |
publicationDate |
2009-12-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2009279872-A |
titleOfInvention |
Fiber absorber and ink tank |
abstract |
PROBLEM TO BE SOLVED: To provide a fiber absorber using a fiber material composed of a core material and a sheath material that is free from elution in ink and can be recycled. SOLUTION: A core material constituting a fiber material having a double structure is made of a polypropylene homopolymer having a melting point of 140 ° C. or higher, and a sheath material has a melting point of less than 140 ° C. and 230 ° C. specified by JIS K7210, 2 It is composed of an ethylene-propylene random copolymer having a melt flow rate measured at 16 kg of 7 g / 10 min or more. [Selection] Figure 6 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9238370-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108481913-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9498964-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2960060-A2 |
priorityDate |
2008-05-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |