http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009275136-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fcc0b66123940d1b32783569ebfa2d45 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L45-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L65-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-04 |
filingDate | 2008-05-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ee8c4114cfa121a81441d71c10c51124 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7e937af2fc3a0e24a0072d19387b621a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_44a5855cdf3fe7c57d6281055c19eb13 |
publicationDate | 2009-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009275136-A |
titleOfInvention | Resin composition for injection molded body formation and injection molded body |
abstract | A resin composition for forming an injection molded body capable of obtaining an injection molded body having a high refractive index, excellent transparency, and excellent durability under high temperature without phase separation during injection molding. And an injection molded body. The weight average molecular weight (Mw) in terms of standard polystyrene measured by gel permeation chromatography (GPC) is 5,000 to 20,000, and the molecular weight distribution (Mw / Mn) is 1.0 to 1. A resin composition for forming an injection-molded article, comprising 1 to 60 parts by weight of polystyrene (A) 5 and 40 to 99 parts by weight of a cyclic olefin-based resin (B). [Selection figure] None |
priorityDate | 2008-05-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links