http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009263566-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F265-06 |
filingDate | 2008-04-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_100baa1a4e3f9f9c91185af6b894486f |
publicationDate | 2009-11-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009263566-A |
titleOfInvention | Method for producing methacrylic resin composition |
abstract | PROBLEM TO BE SOLVED: To provide a methacrylic resin composition having excellent impact resistance and having few defects called fish eyes. SOLUTION: At least one elastic polymer layer obtained by polymerizing a monomer mainly composed of alkyl acrylate and at least one hard polymer obtained by polymerizing a monomer mainly composed of alkyl methacrylate. A polymer (B) obtained by polymerizing a monomer mainly composed of alkyl methacrylate and (A) :( B) = 5: 95 to 70:30 ( (Weight ratio) to the twin-screw kneading extruder, and the motor power consumption (kW) of the extruder / the extrusion amount per unit time of the resin composition extruded from the extruder (kg / h) Melt-kneading is performed so that the specific energy obtained in step 0.10 becomes 0.10 to 0.60 (kW ยท h / kg). [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014024217-A |
priorityDate | 2008-04-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |