http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009253313-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_063a1b324005ddc15e16e7529c6258c4
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G09G2310-066
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G09G3-2932
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01J11-12
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01J11-40
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G09G3-2927
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H04N5-66
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G09G3-288
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G09G3-20
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G09G3-298
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G09G3-296
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G09G3-294
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G09G3-293
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G09G3-292
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G09G3-291
filingDate 2008-04-01-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e71fa9ff9059676736e14c9483bbe5d5
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3d9d43f8cdbaf15c20094f66cf2511e0
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7f7dc59da51d758fecabef18344c434e
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_68b8cb6f48f2b99c61339d52dbfe23e8
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_76a831a69fd4f3e6a79bb3d9868fcfd4
publicationDate 2009-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber JP-2009253313-A
titleOfInvention Plasma display device
abstract A high-definition PDP has a problem that an image display cannot be normally performed due to a defective address operation due to generation of strong discharge in an initialization period and discharge interference between adjacent cells. A plurality of agglomerated particle groups in which a plurality of crystal particles made of metal oxide are aggregated are arranged in the periphery of a protective layer 18, and during the initialization period, the second electrode is gently applied from the first voltage to the second voltage. Image display is performed by a driving method having a first half of an initialization period in which a rising voltage is applied and a second half of an initialization period in which a voltage that gradually falls from the third voltage to the fourth voltage is applied. [Selection] Figure 9
priorityDate 2008-04-01-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008293803-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007311075-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003050563-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006244784-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-0233690-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008021660-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001118511-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008293772-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007035655-A
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/gene/GID10268
http://rdf.ncbi.nlm.nih.gov/pubchem/gene/GID56820
http://rdf.ncbi.nlm.nih.gov/pubchem/gene/GID56089
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419491805
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID5416
http://rdf.ncbi.nlm.nih.gov/pubchem/gene/GID613547
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419569951
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID14792

Total number of triples: 44.